♦Alurinmorin elo Name: Nickel Welding Waya, ErNiCrMo-4 Wire Welding, Hastelloy C276 Welding Waya
♦ MOQ:15kg
♦ Fọọmu: MIG(15kgs/spool), TIG(5kgs/apoti)
♦ Iwọn: Opin 0.01mm-8.0mm
♦ Iwọn ti o wọpọ0.8MM / 1.0MM / 1.2MM / 1.6MM / 2.4MM / 3.2MM / 3.8MM / 4.0MM / 5.0MM
♦ Awọn ajohunše: Ni ibamu si Ijẹrisi AWS A5.14 ASME SFA A5.14
ErNiCrMo-4 ti wa ni lilo fun alurinmorin Hastelloy C276, nickel base alloy ati awọn ohun elo miiran, nickel alloy to irin tabi irin alagbara, irin, tun lo fun alurinmorin nickel CrMo alloy apapo Layer lori steel.Main alurinmorin ohun elo ti iru kemikali tiwqn bi daradara bi dissimilar ohun elo ti nickel mimọ alloys. , irin ati irin alagbara.A tun le lo alloy yii fun didimu irin pẹlu irin nickel-chrome-molybdenum weld.Awọn akoonu molybdenum ti o ga julọ n pese atako nla si idamu ipata aapọn, pitting ati ipata crevice.
C | Cr | Ni | Si | Mn | P | S | Cu | Fe | V | W | Mo | Co |
≤0.02 | 14.5-16.5 | Ba | ≤0.08 | ≤1.0 | ≤0.04 | ≤0.03 | ≤0.5 | 4.0-7.0 | ≤0.35 | 3.0-4.0 | 15.0-17.0 | ≤2.5 |
Iwọn opin | Ilana | Folti | Amps | Gaasi Idaabobo | |
In | mm | ||||
0.035 | 0.9 | GMAW | 26-29 | 150-190 | Sokiri Gbigbe100% Argon |
0.045 | 1.2 | GMAW | 28-32 | 180-220 | |
1/16 | 1.6 | GMAW | 29-33 | 200-250 | |
1/16 | 1.6 | GMAW | 14-18 | 90-130 | 100% Argon |
3/32 | 2.4 | GMAW | 15-20 | 120-175 | 100% Argon |
1/8 | 3.2 | GMAW | 15-20 | 150-220 | 100% Argon |
Ipo | Agbara Fifẹ MPa (ksi) | Agbara ikore MPa (ksi) | Ilọsiwaju% |
AWS atunṣe | 690(100) | Lai so ni pato | Lai so ni pato |
Aṣoju esi bi welded | 730(106) | 540(79) | 39 |
MIG: 75% Ar / 25% Oun
TIG: 100% Ari
Awọn alloy jẹ sooro si acid ati acid vapor corrosion.Nitori ti akoonu molybdenum ti o ga, o ni idiwọ ti o lagbara si wahala ipata kiraki, pitting ati cavitation corrosion
Ti a lo jakejado ni awọn pipeline eiyan kemikali, awọn falifu fifa, ile-iṣẹ agbara eefin gaasi desulfurization ati alurinmorin -196℃ ohun elo ti 9% Ni irin.